HASTELLOY B2 UNS N10665 W.NR.2.4617
Cyfansoddiad Cemegol
aloi | elfen | C | Si | Mn | S | P | Ni | Cr | Mo | Fe | Co |
Aloi B2 | Minnau | 26.0 | |||||||||
Max | 0.02 | 0.10 | 1.00 | 0.03 | 0.04 | Cydbwysedd | 1.0 | 30.0 | 2.0 | 1.0 |
Priodweddau Mecanyddol
Statws Aolly | Cryfder tynnol Rm Mpa Minnau | Cryfder cynnyrch RP 0. 2 Mpa Minnau | Elongation A 5 % Minnau |
Ateb | 745 | 325 | 40 |
Priodweddau Corfforol
Dwysedd g/cm3 | Pwynt Toddi ℃ |
9.2 | 1330 ~ 1380 |
Safonol
Gwialen, Bar, Gwifren a Gofannu Stoc- ASTM B 335 (Gwialen, Bar), ASTM B 564 (Gofannu), ASTM B 366 (Gosod)
Plât, Taflen a Llain— ASTM B 333
Pibell a Thiwb- ASTM B 622 (Di-dor) ASTM B 619/B626 (Tiwb wedi'i Weldio)
Nodweddion Hastelloy B2
● Gwrthwynebiad mawr i straen cracio a thyllu
● Gwrthwynebiad sylweddol i amodau lleihau fel hydrogen clorid, asidau sylffwrig, asetig a ffosfforig
● Ymwrthedd i asid hydroclorig ar bob crynodiad a thymheredd
● Pâr o: ICONEL® aloi C-276 UNS N10276/W.Nr. 2. 4819
● Nesaf: HASTELLOY B-3 UNS N10675/W.Nr.2.4600
Pam Dewiswch Ni:
1. tîm ymchwil a datblygu proffesiynol
Mae cefnogaeth prawf cais yn sicrhau nad ydych chi bellach yn poeni am offerynnau prawf lluosog.
2. Cydweithrediad marchnata cynnyrch
Mae'r cynhyrchion yn cael eu gwerthu i lawer o wledydd ledled y byd.
3. rheoli ansawdd llym
4. Sefydlog amser cyflwyno a Gorchymyn rhesymol rheoli amser cyflwyno.
Rydym yn dîm proffesiynol, mae gan ein haelodau flynyddoedd lawer o brofiad mewn masnach ryngwladol. Rydym yn dîm ifanc, yn llawn ysbrydoliaeth ac arloesedd. Rydym yn dîm ymroddedig. Rydym yn defnyddio cynhyrchion cymwys i fodloni cwsmeriaid ac ennill eu hymddiriedaeth. Rydym yn dîm gyda breuddwydion. Ein breuddwyd gyffredin yw darparu'r cynhyrchion mwyaf dibynadwy i gwsmeriaid a gwella gyda'i gilydd. Ymddiried ynom, ennill-ennill.