  • Nitronig

    Cyfansoddiad cemegol aloi tymheredd uchel Gradd C si mn sp cr ni fe mo ti cu nb n arall ddim yn fwy na nitronic50 0.06 1 4 ~ 6 0.03 0.04 20.5 ~ 23.5 11.5 ~ 13.5 Sylfaen 1.5 ~ 3 - - - 0.1 ~ 0.3 0.2 ~ 00 0.1 3.5~4.5 7~9 0.03 0.04 16~18 8~9 sylfaen — — — — 0.08~0.18 - aloi lleiafswm eiddo Gradd cyflwr cryfder tynnol RmN/m㎡ Cynnyrch Cryfder Rp0.2N/m.
  • Taflen Data Deunydd 17-4PH

    Dynodwyr rhyngwladol

    AISI 630, ASTM A564-89 17-4PH, JIS SCS24 / SUS630, AFNOR Z7CNU15-05 / Z7CNU17-04

  • Aloi Precision Uchel

    Aloi Tymheredd Uchel Cyfansoddiad cemegol Gradd C Si Mn SP Cr Ni Mo Cu Fe Al Co Ti dim mwy na 1J50 0.03 0.15 ~0.3 0.3 ~0.6 0.02 0.02 - 49.5 ~ 50.5 - ≤0.2 sylfaen —0.6 ~ 0.6 — .1 0.02 0.02 - 78.5~80.5 3.8~4.1 ≤0.2 sylfaen — — — 3J53 0.05 0.8 0.8 0.02 0.02 5.2 ~ 5.8 41.5 ~ 40 0.3 ~ .7 4J29 0.03 0.3 0.5 0.02 0.02 ...
  • Nicel

    Aloi Tymheredd Uchel Cyfansoddiad cemegol Gradd Ni Fe Cu C Mn S Si Nickel200 99 ≤0.4 ≤0.25 ≤0.15 ≤0.35 ≤0.01 ≤0.35 Nickel201 99 ≤0.4 ≤0.20 ≤ ≤0.03 ≤0.20 0.35 aloi eiddo isafswm ffurf cynnyrch cyflwr cryfder tynnol RmN /m㎡ Cryfder Cynnyrch Rp0.2N/m㎡ Elongation Fel% caledwch Brinell HB ffon a stribed wedi'i rolio'n boeth 60~85 15~45 35~55 45~80 ffon a stribed oer wedi'i dynnu neu ei anelio 55~75 15...
  • Dur Di-staen Biphase

    Aloi Tymheredd Uchel Cyfansoddiad cemegol Gradd C Si Mn SP Cr Ni Mo Cu NW arall dim mwy na F51 0.03 1 2 0.02 0.03 21~23 4.5~6.5 2.5~3.5 - 0.08 ~ 0.2 - - F353 0.03 0.03 0.0 - 0.03 . ~ 26 6 ! .035 23~28 3~6 1 ~3 - - - - A4 ...