Monel 400 Uns N04400 W.Nr.2.4360 A 2.4361
Cyfansoddiad Cemegol
aloi | elfen | C | Si | Mn | S | Ni | Fe | Cu |
Monel 400 | Minnau | 63.0 | 28.0 | |||||
Max | 0.3 | 0.5 | 2.0 | 0.024 | 2.5 | 34.0 |
Priodweddau Mecanyddol
Statws Aolly | Cryfder tynnol Rm Mpa Minnau | Cryfder cynnyrch RP 0. 2 Mpa Minnau | Elongation A 5 % Minnau |
Ateb | 745 | 325 | 40 |
Priodweddau Corfforol
Statws Aolly | Cryfder tynnol Rm Mpa Min. | Nerth cynnyrch RP 0. 2 Mpa Min. | Elongation A 5 % |
annealed | 480 | 170 | 35 |
Safonol
Gwialen, Bar, Gwifren a Gofannu Stoc- ASTM B 164 (Gwialen, Bar, a Gwifren), ASTM B 564 (Gofaniadau)
Plât, Taflen a Llain-,ASTM B 127, ASME SB 127
Pibell & Tiwb- ASTM B 165 (Pibell a thiwb di-dor), ASTM B 725 (Pibell Weldiedig), ASTM B 730 (Tiwb Wedi'i Weldio), ASTM B 751 (Tiwb Wedi'i Weldio), ASTM B 775 (Pibell Weldiedig), ASTM B 829 (Pibell Ddi-dor a Tiwb)
Cynhyrchion Weldio- Metel Llenwi 60-AWS A5.14 / ERNiCu-7; Electrod Weldio 190-AWS A5.11 / ENiCu-7.
Nodweddion Monel 400
● Yn gwrthsefyll dŵr môr a stêm ar dymheredd uchel
● Gwrthwynebiad ardderchog i ddŵr hallt neu ddŵr môr sy'n llifo'n gyflym
● Gwrthwynebiad ardderchog i gracio cyrydiad straen yn y rhan fwyaf o ddyfroedd croyw
● Yn arbennig o ymwrthol i asidau hydroclorig a hydrofflworig pan gânt eu dad-awyru
● Yn cynnig rhywfaint o wrthwynebiad i asidau hydroclorig a sylffwrig ar dymheredd a chrynodiadau cymedrol, ond anaml y mae'n ddeunydd o ddewis ar gyfer yr asidau hyn
● Gwrthwynebiad ardderchog i halen niwtral ac alcalïaidd
● Gwrthwynebiad i gracio cyrydiad straen a achosir gan glorid
● Priodweddau mecanyddol da o dymheredd is-sero hyd at 1020 ° F
● Gwrthwynebiad uchel i alcalïau
● Pâr o: Alloy N-155